Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 0.00133 bar @Temperature 48.0 °C |
1.00 torr @Temperature 118 °F |
|
Indium Corp. GaCl3 Gallium Trichloride, Anhydrous Synonyms: Gallium Chloride, Gallium (III) ChlorideCAS Number: 13450-90-3EC Number: 236-610-0RTECS: LW9100000Purity: 99.5 to 99.999% Gallium TrichlorideAppearance: Clear or White, Needle-shaped.. |
|||
Vapor Pressure | 0.00133 bar @Temperature 80.0 °C |
0.996 torr @Temperature 176 °F |
|
Solvay Chemicals Glycerol alpha monochlorohydrin Viscous liquid used as chemical intermediate.EINECS Number: 202-492-4/CAS Number: 96-24-2/UN number: 2689Information provided by Solvay |
|||
Vapor Pressure | 0.00133 bar @Temperature 0.000 °C |
1.00 torr @Temperature 32.0 °F |
|
Solvay Specialty Polymers Galden® SV135 PFPE Solvent Galden® SV grades are specifically recommended for use as solvents.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service temperature.. |
|||
Vapor Pressure | <= 0.00133 bar @Temperature 180 °C |
<= 1.00 torr @Temperature 356 °F |
AboCast |
Abatron AboCast/AboCure 8109-1 High melting point.Processing: 100/30 pbw; mix at 130-140°C (270 °F); cures in 16 h/120°C (250°F), 10 h/140°C (285°F), 8 h/160°C (320°F), 2 h/ 200°C (390°F).Applications: Heavy duty castin.. |
|||
Vapor Pressure | 0.00133 bar @Temperature 100 °C |
1.00 torr @Temperature 212 °F |
AboCure |
Abatron AboCast/AboCure 8109-1 High melting point.Processing: 100/30 pbw; mix at 130-140°C (270 °F); cures in 16 h/120°C (250°F), 10 h/140°C (285°F), 8 h/160°C (320°F), 2 h/ 200°C (390°F).Applications: Heavy duty castin.. |
|||
Vapor Pressure | 0.00133 bar @Temperature 180 °C |
1.00 torr @Temperature 356 °F |
AboCast |
Abatron AboCast/AboCure 8109-10 2-part, clear, slow casting/impregnating dielectric compound. Low dielectric constant, good flexibility and thermocycling properties. Abocast 8502-4 is a red (and other colors), filled version.Pro.. |
|||
Vapor Pressure | 0.00133 bar @Temperature 100 °C |
1.00 torr @Temperature 212 °F |
AboCure |
Abatron AboCast/AboCure 8109-10 2-part, clear, slow casting/impregnating dielectric compound. Low dielectric constant, good flexibility and thermocycling properties. Abocast 8502-4 is a red (and other colors), filled version.Pro.. |
|||
Vapor Pressure | 0.00133 bar @Temperature 180 °C |
1.00 torr @Temperature 356 °F |
AboCast |
Abatron AboCast/AboCure 8109-11 All-purpose, structural dielectric resin. Better thermal and chemical properties than 8109-8, but requires heat cure. Melts at 70-80°C and remains liquid (supercooled) for many hours at RT.Process.. |
|||
Vapor Pressure | 0.00133 bar @Temperature 180 °C |
1.00 torr @Temperature 356 °F |
AboCast |
Abatron AboCast/AboCure 8109-12 1-part, contains latent hardener activated by higher temperature. 4-6 month shelf life at 20-25°C (68-77°F). Other versions available with longer shelf lives and cure cycles.Processing: Potlife:.. |
|||
Vapor Pressure | <= 0.00133 bar @Temperature 180 °C |
<= 1.00 torr @Temperature 356 °F |
AboCast |
Abatron AboCast/AboCure 8109-2 High melting point. Filled version.Processing: 100/10 pbw; 90 minute potlife; mix at 130-140°C (270 °F); cures in 16 h/120°C (250°F), 10 h/140°C (285°F), 8 h/160°C (320°F), 2 h/ 200°C (390°.. |
|||
Vapor Pressure | 0.00133 bar @Temperature 100 °C |
1.00 torr @Temperature 212 °F |
AboCure |
Abatron AboCast/AboCure 8109-2 High melting point. Filled version.Processing: 100/10 pbw; 90 minute potlife; mix at 130-140°C (270 °F); cures in 16 h/120°C (250°F), 10 h/140°C (285°F), 8 h/160°C (320°F), 2 h/ 200°C (390°.. |
|||
Vapor Pressure | <= 0.00133 bar @Temperature 100 °C |
<= 1.00 torr @Temperature 212 °F |
AboCast |
Abatron AboCast/AboCure 8109-3 Low viscosity, RT cure. Easy processing.Processing: 100/10 pbw; Potlife: 2.5 h/20°C (68°F), 30 min/40°C (105°F), 15 min/60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 h/60°C (140.. |
|||
Vapor Pressure | <= 0.00133 bar @Temperature 100 °C |
<= 1.00 torr @Temperature 212 °F |
AboCast |
Abatron AboCast/AboCure 8109-4 Safety hardener (minimum toxicity) version of 8109-3.Processing: 100/10 pbw; Potlife: 2.5 h/20°C (68°F), 30 min/40°C (105°F), 15 min/60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 .. |
|||
Vapor Pressure | <= 0.00133 bar @Temperature 180 °C |
<= 1.00 torr @Temperature 356 °F |
AboCast |
Abatron AboCast/AboCure 8109-5 High heat resistance. Easy to use.Processing: 100/20 pbw; Potlife: 7-10 days/20°C (68°F), 5-7h/60°C (140°F); mix at RT; cures in: 4 h/100°C (212°F) + 3 h/190°C (375°F) postcure.Applications.. |
|||
Vapor Pressure | <= 0.00133 bar @Temperature 180 °C |
<= 1.00 torr @Temperature 356 °F |
AboCast |
Abatron AboCast/AboCure 8109-6 High heat resistance. Easy to use.Processing: 100/90 pbw; Potlife: 15-20 days/20°C (68°F), 7-10 h/120°C (250°F); mix at RT; cures in: 3 h/100°C (212°F) + 3 h/190°C (375°F) postcure.Applicat.. |
|||
Vapor Pressure | 0.00133 bar @Temperature 180 °C |
1.00 torr @Temperature 356 °F |
AboCast |
Abatron AboCast/AboCure 8109-8 All-purpose, structural dielectric resin. High thermal and chemical resistance and RT cure.Processing: 100/12 ratio; Potlife: 45 min/20°C (68°F), 20 min/40°C (105°F), 10 min /60°C (140°F); mi.. |
|||
Vapor Pressure | 0.00133 bar @Temperature 180 °C |
1.00 torr @Temperature 356 °F |
AboCast |
Abatron AboCast/AboCure 8109-9 Minimum toxicity version of 8109-8.Processing: 100/25 ratio; Potlife: 45 min/20°C (68°F), 20 min/40°C (105°F), 10 min /60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 h/60°C (140°.. |
|||
Vapor Pressure | <= 0.00133 bar @Temperature 180 °C |
<= 1.00 torr @Temperature 356 °F |
AboCast |
Abatron AboCast/AboCure 8109-7 Processing: 100/80 pbw; Potlife: 6-7 days/20°C (68°F), 12-24 h/40°C (105°F), 0.75-7 h /60°C (140°F); mix at 50-80°C (120-175°F); cures in: 1 h/100°C (212°F) + 4 h/150°C (300°F) postcure... |