Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.81 g/cc @Temperature 20.0 °C |
0.282 lb/in³ @Temperature 68.0 °F |
Hardened and tempered to 310 HB |
EDRO #3 Prehardened Mold Quality P20 Alloy Steel EDRO #3™ is a vacuum-degassed, ladle refined, Cr-Ni-Mo- alloyed steel which is supplied in the hardened and tempered condition. EDRO #3™ is manufactured to consistently high quality standards with.. |
|||
Density | 7.81 g/cc @Temperature 20.0 °C |
0.282 lb/in³ @Temperature 68.0 °F |
Hardened and tempered to 57 HRC |
EDRO #7 Shock Resistant S7 Tool Steel EDRO #7™ is a chromium-molybdenum steel characterized by: high toughness, good wear resistance, high impact resistance, good through hardening properties, good machinability, and good dimensional s.. |
|||
Density | 7.81 g/cc @Temperature 20.0 °C |
0.282 lb/in³ @Temperature 68.0 °F |
Hardened and tempered to 50 HRC |
EDRO #8 Premium 420 Stainless Mold Steel EDRO #8™ is a chromium-alloyed stainless tool steel with the following properties: excellent corrosion resistance, superior polishability, good wear resistance, good machinability, and stability in.. |
|||
Density | 7.81 g/cc @Temperature 199 °C |
0.282 lb/in³ @Temperature 390 °F |
|
EDRO EDRO400™ #40 Prehardened Insert Quality Martensitic Stainless Steel EDRO400™ is a remelted 400 series martensitic stainless steel supplied prehardened to 40 HRC (375 HB).EDRO400™ is characterized by excellent polishability, superior corrosion resistance, high leve.. |
|||
Density | 7.81 g/cc @Temperature 199 °C |
0.282 lb/in³ @Temperature 390 °F |
Prehardened to 293 HB |
EDRO P1FM #31 Free Machining Holder Steel EDRO #31 P1-FM is a free machining low alloy steel supplied prehardened to 262-321 HB.P1-FM is characterized by excellent machinability, uniform and consistent hardness in all dimensions, good resis.. |
|||
Density | 7.81 g/cc @Temperature 199 °C |
0.282 lb/in³ @Temperature 390 °F |
Prehardened to 321 HB |
EDRO RoyAlloy™ #6 Free Machining Stainless Holder Steel RoyAlloy™ is a 400 series martensitic stainless steel supplied prehardened. RoyAlloy™ is characterized by excellent machinability, good corrosion resistance, uniform and consistent hardness in all.. |
|||
Density | 7.81 g/cc @Temperature 199 °C |
0.282 lb/in³ @Temperature 390 °F |
Age-hardened to 42 HRC |
EDRO UltraChem® #15 Precipitation Hardening Stainless Mold Steel Ultrachem® is a chromium-nickel precipitation-hardening stainless steel, a modified PH alloy grade, which is characterized by: exceptional corrosion resistance, uniform hardness in all dimensions, .. |
|||
Density | 7.81 g/cc @Temperature 199 °C |
0.282 lb/in³ @Temperature 390 °F |
Prehardened to 321 HB |
EDRO UltraChem® ESR #16 Precipitation Hardening Stainless Mold Steel Ultrachem ESR® is a chromium-nickel precipitation-hardening stainless steel, a modified PH alloy grade, which is characterized by exceptional polishability, exceptional corrosion resistance, unifor.. |