Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.943 - 0.951 g/cc @Temperature 23.0 °C |
0.0341 - 0.0344 lb/in³ @Temperature 73.4 °F |
|
Kazanorgsintez PE80B-275 Medium Density Polyethylene Composite Production Method: Copolymerization of ethylene at low pressure using advanced technology and in presence of complex catalysts on carrier material that allows production of polyethylene with enhanc.. |
|||
Density | 0.943 - 0.951 g/cc @Temperature 23.0 °C |
0.0341 - 0.0344 lb/in³ @Temperature 73.4 °F |
|
Kazanorgsintez PE80B-286 Medium Density Polyethylene Composite Production Method: Copolymerization of ethylene at low pressure using advanced technology and in presence of complex catalysts on carrier material that allows production of polyethylene with enhanc.. |