Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.86 g/cc @Temperature 20.0 °C |
0.284 lb/in³ @Temperature 68.0 °F |
|
EDRO EDRO400™ #40 Prehardened Insert Quality Martensitic Stainless Steel EDRO400™ is a remelted 400 series martensitic stainless steel supplied prehardened to 40 HRC (375 HB).EDRO400™ is characterized by excellent polishability, superior corrosion resistance, high leve.. |
|||
Density | 7.86 g/cc @Temperature 20.0 °C |
0.284 lb/in³ @Temperature 68.0 °F |
Prehardened to 293 HB |
EDRO P1FM #31 Free Machining Holder Steel EDRO #31 P1-FM is a free machining low alloy steel supplied prehardened to 262-321 HB.P1-FM is characterized by excellent machinability, uniform and consistent hardness in all dimensions, good resis.. |
|||
Density | 7.86 g/cc @Temperature 20.0 °C |
0.284 lb/in³ @Temperature 68.0 °F |
Prehardened to 321 HB |
EDRO RoyAlloy™ #6 Free Machining Stainless Holder Steel RoyAlloy™ is a 400 series martensitic stainless steel supplied prehardened. RoyAlloy™ is characterized by excellent machinability, good corrosion resistance, uniform and consistent hardness in all.. |
|||
Density | 7.86 g/cc @Temperature 20.0 °C |
0.284 lb/in³ @Temperature 68.0 °F |
Age-hardened to 42 HRC |
EDRO UltraChem® #15 Precipitation Hardening Stainless Mold Steel Ultrachem® is a chromium-nickel precipitation-hardening stainless steel, a modified PH alloy grade, which is characterized by: exceptional corrosion resistance, uniform hardness in all dimensions, .. |
|||
Density | 7.86 g/cc @Temperature 20.0 °C |
0.284 lb/in³ @Temperature 68.0 °F |
Prehardened to 321 HB |
EDRO UltraChem® ESR #16 Precipitation Hardening Stainless Mold Steel Ultrachem ESR® is a chromium-nickel precipitation-hardening stainless steel, a modified PH alloy grade, which is characterized by exceptional polishability, exceptional corrosion resistance, unifor.. |
|||
Density | 7.85 g/cc @Temperature 20.0 °C |
0.284 lb/in³ @Temperature 68.0 °F |
|
Bohler-Uddeholm BÖHLER W303 ISODISC® Hot Work Tool Steel Description: Hot work tool steel featuring excellent hot tensile properties, high retention of hardness, good toughness and resistance to heat checking, admits water cooling. BOHLER W303 is also ava.. |
|||
Density | 7.85 g/cc @Temperature 20.0 °C |
0.284 lb/in³ @Temperature 68.0 °F |
|
Bohler-Uddeholm BÖHLER W403 VMR® Hot Work Tool Steel W403 VMR is a modified hot work alloy with an excellent combination of hot tensile properties and toughness. The balanced properties of this grade are not only due to chemistry modification, but to .. |