Physical Properties Metric English Comments
Density 7.81 g/cc

@Temperature 20.0 °C
0.282 lb/in³

@Temperature 68.0 °F
Hardened and tempered to 310 HB
EDRO #3 Prehardened Mold Quality P20 Alloy Steel
EDRO #3™ is a vacuum-degassed, ladle refined, Cr-Ni-Mo- alloyed steel which is supplied in the hardened and tempered condition. EDRO #3™ is manufactured to consistently high quality standards with..
Density 7.81 g/cc

@Temperature 20.0 °C
0.282 lb/in³

@Temperature 68.0 °F
Hardened and tempered to 57 HRC
EDRO #7 Shock Resistant S7 Tool Steel
EDRO #7™ is a chromium-molybdenum steel characterized by: high toughness, good wear resistance, high impact resistance, good through hardening properties, good machinability, and good dimensional s..
Density 7.81 g/cc

@Temperature 20.0 °C
0.282 lb/in³

@Temperature 68.0 °F
Hardened and tempered to 50 HRC
EDRO #8 Premium 420 Stainless Mold Steel
EDRO #8™ is a chromium-alloyed stainless tool steel with the following properties: excellent corrosion resistance, superior polishability, good wear resistance, good machinability, and stability in..
Density 7.81 g/cc

@Temperature 199 °C
0.282 lb/in³

@Temperature 390 °F
EDRO EDRO400™ #40 Prehardened Insert Quality Martensitic Stainless Steel
EDRO400™ is a remelted 400 series martensitic stainless steel supplied prehardened to 40 HRC (375 HB).EDRO400™ is characterized by excellent polishability, superior corrosion resistance, high leve..
Density 7.81 g/cc

@Temperature 199 °C
0.282 lb/in³

@Temperature 390 °F
Prehardened to 293 HB
EDRO P1FM #31 Free Machining Holder Steel
EDRO #31 P1-FM is a free machining low alloy steel supplied prehardened to 262-321 HB.P1-FM is characterized by excellent machinability, uniform and consistent hardness in all dimensions, good resis..
Density 7.81 g/cc

@Temperature 199 °C
0.282 lb/in³

@Temperature 390 °F
Prehardened to 321 HB
EDRO RoyAlloy™ #6 Free Machining Stainless Holder Steel
RoyAlloy™ is a 400 series martensitic stainless steel supplied prehardened. RoyAlloy™ is characterized by excellent machinability, good corrosion resistance, uniform and consistent hardness in all..
Density 7.81 g/cc

@Temperature 199 °C
0.282 lb/in³

@Temperature 390 °F
Age-hardened to 42 HRC
EDRO UltraChem® #15 Precipitation Hardening Stainless Mold Steel
Ultrachem® is a chromium-nickel precipitation-hardening stainless steel, a modified PH alloy grade, which is characterized by: exceptional corrosion resistance, uniform hardness in all dimensions, ..
Density 7.81 g/cc

@Temperature 199 °C
0.282 lb/in³

@Temperature 390 °F
Prehardened to 321 HB
EDRO UltraChem® ESR #16 Precipitation Hardening Stainless Mold Steel
Ultrachem ESR® is a chromium-nickel precipitation-hardening stainless steel, a modified PH alloy grade, which is characterized by exceptional polishability, exceptional corrosion resistance, unifor..
Density 7.80 g/cc

@Temperature 20.0 °C
0.282 lb/in³

@Temperature 68.0 °F
Bohler-Uddeholm BÖHLER W302 SUPERIOR® Premium H13 Tool Steel
A premium grade H13 hot work tool steel featuring:Very good toughness properties meeting the requirements of NADCA 207-97, and the superior quality levels of NADCA 207-2003Very good heat checking re..
Density 7.80 g/cc

@Temperature 20.0 °C
0.282 lb/in³

@Temperature 68.0 °F
Bohler-Uddeholm BÖHLER W400 VMR® H11 Hot Work Tool Steel
W400 VMR is a low silicon, chromium-vanadium hot work tool steel which has been vacuum remelted to obtain the highest uniformity, the best cleanliness of tool steel. The material is characterized:E..
Density 7.80 g/cc

@Temperature 20.0 °C
0.282 lb/in³

@Temperature 68.0 °F
Bohler-Uddeholm BÖHLER W302 ISOBLOC® H13 hot work tool steel
Properties:Hot work tool steel featuring excellent hot tensile properties, high hot wear resistance, adequate toughness and heat checking resistance, adequate toughness and heat checking; admits wat..