Physical Properties | Metric | English | Comments |
---|---|---|---|
Volatile Organic Compounds (VOC) Content | 80 g/l | 80 g/l | |
Dow Corning 772 WATER REPELLENT Dow Corning® 777 Water Repellent is a water-dilutable solution of potassium methyl siliconate designed to impart water repellency to a wide variety of surfaces. Supplied at a concentration of 40 pe.. |
|||
Volatile Organic Compounds (VOC) Content | <= 80 g/l | <= 80 g/l | US EPA |
Chesterton 294 CSD Industrial Degreaser Description: Chesterton® 294 CSD is a fast acting, industrial degreaser for critical equipment. It contains no chlorinate, aromatic or solvents of questionable toxicity. Designed to quickly penetra.. |
|||
Volatile Organic Compounds (VOC) Content | <= 80 g/l | <= 80 g/l | |
3M Hi-Strength 94 ET Adhesive A high performance, industrial grade spray adhesive with a unique low telegraphing pebble spray pattern.Features:Bonds to a variety of substrates including decorative laminate, headliners, and soft .. |
|||
Volatile Organic Compounds (VOC) Content | <= 80 g/l | <= 80 g/l | |
3M Hi-Strength 94 ET Cylinder Spray Adhesive A high performance, industrial grade spray adhesive with a unique low telegraphing pebble spray pattern.Features:Bonds to a variety of substrates including decorative laminate, headliners, and soft .. |
|||
Volatile Organic Compounds (VOC) Content | <= 80 g/l | <= 80 g/l | |
3M Scotch-Weld™ General Purpose 60 CA Adhesive A low VOC general purpose industrial grade spray adhesiveFeatures:This adhesive brings value as it has exceptionally high solidsThis adhesive is designed for temporary or permanent bonds on substrat.. |
|||
Volatile Organic Compounds (VOC) Content | <= 80 g/l | <= 80 g/l | |
3M Scotch-Weld™ General Purpose 60 CA Cylinder Spray Adhesive A low VOC general purpose industrial grade spray adhesiveFeatures:This adhesive brings value as it has exceptionally high solidsThis adhesive is designed for temporary or permanent bonds on substrat.. |
|||
Volatile Organic Compounds (VOC) Content | <= 80 g/l | <= 80 g/l | |
3M Scotch-Weld™ Hi-Strength Postforming 94 CA Cylinder Spray Adhesive A low VOC, high performance, postformable grade spray adhesive with a unique low telegraphing pebble spray pattern.Features:Bonds to a variety of demanding substrates like decorative laminate, metal.. |
|||
Volatile Organic Compounds (VOC) Content | <= 80 g/l | <= 80 g/l | |
3M Scotch-Weld™ Hi-Strength Postforming 94 CA Spray Adhesive A low VOC, high performance, postformable grade spray adhesive with a unique low telegraphing pebble spray pattern.Features:Bonds to a variety of demanding substrates like decorative laminate, metal.. |