Polymer Property : Volatile Organic Compounds (VOC) Content = 773 g/l Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content 773 g/l
773 g/l
Mixed; ASTM D3960-87
Lord Adhesives Aeroglaze® 9924V Wash Primer
Aeroglaze® 9924V wash primer was designed for priming metal surfaces. It is particularly useful for priming non-ferrous substrates such as aluminum and galvanized steel.All information provided b..