Polymer Property : Volatile Organic Compounds (VOC) Content = 73 g/l Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content 73 g/l
73 g/l
Dow Corning Z-6689 WATER REPELLENT
Dow Corning® Z-6689 Water Repellent is a solvent-free silane/ siloxane concentrate, dilutable in organic or silicone solvents to formulate a water repellent. Upon proper application, the formulated..