Physical Properties | Metric | English | Comments |
---|---|---|---|
Volatile Organic Compounds (VOC) Content | 520 g/l | 520 g/l | ASTM D3960-87 |
Lord Adhesives Aeroglaze® A276 Reflective Polyurethane Aeroglaze® A276 reflective polyurethane gives a hard, flexible, colorfast, non-chalking surface that is resistant to most acids, alkaline detergents, lubricants, and chemicals.All information provi.. |