Physical Properties | Metric | English | Comments |
---|---|---|---|
Volatile Organic Compounds (VOC) Content | 12.93 g/l | 12.93 g/l | |
Tra-Con Tra-Bond FS469 Clear High Strength Epoxy TRA-BOND FS469 is a clear low viscosity epoxy formulation designed for bonding and coating micro-electronics, laminations, optical components and laser assemblies. The low cure shrinkage (using a ro.. |