Physical Properties | Metric | English | Comments |
---|---|---|---|
Storage Temperature | <= 30.0 °C | <= 86.0 °F | |
Dow Corning SYL-OFF® 7600 COATING Syl-off® 7600 coating is a 100% active solids, pre-catalysed, coating containing a medium viscosity vinyl endblocked and pendant functional silicone polymer.Information provided by Dow Corning |
|||
Storage Temperature | <= 30.0 °C | <= 86.0 °F | |
Dow Corning SYL-OFF® 7673 COATING Syl-Off® 7673 Coating is a 100% active solids pre-catalysed, coating containing a medium viscosity vinyl endblocked only functional silicone polymer. Provides a particularly smooth, premium release.. |
|||
Storage Temperature | <= 30.0 °C | <= 86.0 °F | |
Dow Corning SYL-OFF® 7676 RELEASE COATING Syl-Off® 7676 Coating is a 100% active solids, pre-catalysed, coating containing a medium viscosity hexenyl endblocked and pendant functional silicone polymer. Recommended for use against aggressiv.. |
|||
Storage Temperature | <= 30.0 °C | <= 86.0 °F | |
Dow Corning SYL-OFF® 7677 RELEASE COATING Syl-Off® 7677 Coating is a 100% active solids pre-catalysed, coating containing a medium viscosity hexenyl endblocked only functional silicone polymer. Recommended for use against aggressive adhesi.. |
|||
Storage Temperature | <= 30.0 °C | <= 86.0 °F | |
Dow Buna® SB 1712 Cold polymerized Emulsion Styrene Butadiene Rubber (E-SBR) Buna® SB 1712 - Schkopau is manufactured by cold polymerization using mixed rosin acid / fatty acid soaps. It is plasticized with 37.5 parts of an aromatic oil in relation to solid rubber. A disc.. |
|||
Storage Temperature | <= 30.0 °C | <= 86.0 °F | |
Dow Buna® SB 1721 Cold polymerized Emulsion Styrene Butadiene Rubber (E-SBR) Buna® SB 1721 - Schkopau is manufactured by cold polymerization using mixed rosin acid / fatty acid soaps. It is plasticized with 37.5 parts of an aromatic oil in relation to solid rubber. A disc.. |
|||
Storage Temperature | <= 30.0 °C | <= 86.0 °F | |
Dow Buna® SB 1723 Cold polymerized Emulsion Styrene Butadiene Rubber (E-SBR) Buna® SB 1723 - Schkopau is manufactured by cold polymerization using mixed rosin acid / fatty acid soaps. It is plasticized with 37.5 parts of a TDAE oil in relation to solid rubber. A discolori.. |
|||
Storage Temperature | <= 30.0 °C | <= 86.0 °F | |
Dow Buna® SB 1739 Cold polymerized Emulsion Styrene Butadiene Rubber (E-SBR) Buna® SB 1739 - Schkopau is manufactured by cold polymerization using mixed rosin acid / fatty acid soaps. It is plasticized with 37.5 parts of a TDAE oil in relation to solid rubber. A discolori.. |
|||
Storage Temperature | <= 30.0 °C | <= 86.0 °F | |
Dow SE BR-1202C Stereospecific high cis-1,4 Polybutadiene (BR) SE BR-1202C is manufactured by a solution process using cobalt catalyst which produces polymers with a very light color and low level of impurities. A non-staining stabilizer is added during the pr.. |
|||
Storage Temperature | <= 30.0 °C | <= 86.0 °F | |
Dow SE BR-1202D Stereospecific high cis-1,4 Polybutadiene (BR) SE BR-1202D is manufactured by a solution process using cobalt catalyst which produces polymers with a very light color and low level of impurities. A non-staining stabilizer is added during the pr.. |
|||
Storage Temperature | <= 30.0 °C | <= 86.0 °F | |
Dow SE BR-1203H Stereospecific high cis-1,4 Polybutadiene (BR) SE BR-1203H is manufactured by a solution process using cobalt catalyst which produces polymers with a very light color and low ash content. A non-staining stabilizer is added during the production.. |
|||
Storage Temperature | <= 30.0 °C | <= 86.0 °F | |
Dow SE SLR-4601 Solution polymerized Styrene Butadiene Rubber (S-SBR) SE SLR-4601 is manufactured by anionic solution polymerization using lithium initiator. It is a product with medium styrene and high vinyl content. The product is partially Sn-coupled and chemical.. |
|||
Storage Temperature | <= 30.0 °C | <= 86.0 °F | |
Dow SE SLR-4610 H Solution polymerized Styrene Butadiene Rubber (S-SBR) SE SLR-4610 H is manufactured by anionic solution polymerization using lithium initiator and is extended with 37.5 parts of aromatic oil in relation to solid rubber. It is a product with medium sty.. |
|||
Storage Temperature | <= 30.0 °C | <= 86.0 °F | |
Dow SE SLR-4610 Solution polymerized Styrene Butadiene Rubber (S-SBR) SE SLR-4610 is manufactured by anionic solution polymerization using lithium initiator and is extended with 37.5 parts of aromatic oil in relation to solid rubber. It is a product with medium styre.. |
|||
Storage Temperature | <= 30.0 °C | <= 86.0 °F | |
Dow SE BR-1220M Stereospecific high cis-1,4 Polybutadiene (BR) SE BR-1220M is manufactured by a solution process using cobalt catalyst which produces polymers with a very light color and low ash content. A non-staining stabilizer is added during the production.. |
|||
Storage Temperature | <= 30.0 °C | <= 86.0 °F | |
Akzo Nobel Trigonox® D-C50 Polymerization Initiator Initiator for the (co)polymerization of ethylene, styrene, acrylonitrile, acrylates and methacrylates. Trigonox D-C50 may also be used as an initiator for curing unsaturated polyester and vinylester.. |
|||
Storage Temperature | <= 30.0 °C | <= 86.0 °F | |
Akzo Nobel Trigonox® D-E50 Polymerization Initiator Initiator for the (co)polymerization of ethylene, styrene, acrylonitrile, acrylates and methacrylates.Chemical Description: 2,2-Di(tert-butylperoxy)butane, 50% solution in mineral oilCAS Number: 216.. |
|||
Storage Temperature | <= 30.0 °C | <= 86.0 °F | |
Akzo Nobel Trigonox® TAHP-W85 Polymerization Initiator Initiator for the (co)polymerization of styrene, acrylonitrile, acrylates and methacrylates.Chemical Description: tert-Amylhydroperoxide, 85% solution in waterCAS Number: 3425-61-4Acronym: TAHP; Tx .. |
|||
Storage Temperature | >= 30.0 °C | >= 86.0 °F | |
BASF Palamoll® 656 Polymeric Plasticizer Description: Palamoll® 656 is a high viscosity polymeric plasticizer that is compatible with PVC. It is based on adipic acid and polyhydric alcohols. It is resistant to oils, fats, aliphatic hydro.. |