Polymer Property : Relative Viscosity = 3.3 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Relative Viscosity 3.3 cP
3.3 cP
ISO Test; 96 % SAV
BASF Ultramid® C33 01 PA66/6 (Conditioned)
Ultramid C33 01 is an intermediate viscosity PA6/66 grade. Its lower melting point than standard PA6 is advantageous for coextrusion with temperature sensitive polymers like EVOH. It conforms to F..
Relative Viscosity 3.3 cP
3.3 cP
ISO Test; 96 % SAV
BASF Ultramid® C33L 01 PA66/6 (Dry)
Ultramid C33L 01 is an intermediate viscosity, copolymer 6/66.Its lower melting point than standard PA6 is advantageous for coextrusion with temperature sensitive polymers like EVOH. It conforms to..
Relative Viscosity 3.3 cP
3.3 cP
ISO Test; 96 % SAV
BASF Ultramid® C33LN 01 PA66/6 (Dry)
Ultramid C33LN 01 is an intermediate viscosity, copolymer PA6/66 grade. Its lower melting point than standard PA6 is advantageous for coextrusion with temperature sensitive polymers like EVOH. It ..
Relative Viscosity 3.3 cP
3.3 cP
ISO Test; 96 % SAV
BASF Ultramid® B33 01 PA6 (Dry)
Ultramid B33 01 is an intermediate viscosity. PA6 grade. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation "X Polyamide", 1.6.1998 or..
Relative Viscosity 3.3 cP
3.3 cP
ISO Test; 96 % SAV
BASF Ultramid® B33LN 01 PA6 (Dry)
Ultramid B33LN 01 is an intermediate viscosity, PA6 grade. Clarity and thermoformability are enhanced by the incorporation of nucleating and slip agent. It conforms to FDA requirements including, ..
Relative Viscosity 3.3 cP
3.3 cP
ISO Test; 96 % SAV
BASF Ultramid® C33 01 PA66/6 (Dry)
Ultramid C33 01 is an intermediate viscosity PA6/66 grade. Its lower melting point than standard PA6 is advantageous for coextrusion with temperature sensitive polymers like EVOH. It conforms to F..