Physical Properties | Metric | English | Comments |
---|---|---|---|
Relative Viscosity | 3.04 cP | 3.04 cP | Correlation, Cyclohexanone 1%; Internal Method |
PolyOne Geon™ 170 Series 171 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 171 is an ultra-high molecular weight, fine particle size homopolymer dispersion resin intended for use in thin, organosol cast coatings and films. This resin provides excellent fused film an.. |
|||
Relative Viscosity | 3.04 cP | 3.04 cP | Correlation, Cyclohexanone 1%; Internal Method |
PolyOne Geon™ 170 Series 4195 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 171 is an ultra-high molecular weight, fine particle size homopolymer dispersion resin intended for use in thin, organosol cast coatings and films. This resin provides excellent fused film an.. |
|||
Relative Viscosity | 3.04 cP | 3.04 cP | Correlation, Cyclohexanone 1%; Internal Method |
PolyOne Geon™ 170 Series L140UF Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Ultrafine 170-L140UF is an ultra high molecular weight, ultrafine particle size homopolymer dispersion resin. The excellent dispersibility provides good product throughput during the organoso.. |