Physical Properties | Metric | English | Comments |
---|---|---|---|
Relative Viscosity | 1.83 cP | 1.83 cP | QC-10-104 |
Formosa Plastics Formolon® 186 PVC PVC Copolymer Suspension Resin F-186 is a medium molecular vinyl chloride/vinyl acetate copolymer suspension resin. This resin is primarily used in the calendaring and extrusion of rigid film F-186 .. |
|||
Relative Viscosity | 1.83 cP | 1.83 cP | QC-10-104 |
Formosa Plastics Formolon® 172 PVC PVC Copolymer Suspension Resin F-172 is a medium molecular vinyl chloride/vinyl acetate copolymer suspension resin. This resin is primarily used in the calendaring and extrusion of rigid film F-172 .. |