Polymer Property : Melt Index of Compound = 9.0 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Index of Compound 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® FST9436 PC Copolymer
Medium viscosity opaque, low smoke, and OSU 65/65 compliant PC Copolymer
Melt Index of Compound 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF0335 PC (Europe-Africa-Middle East)
LNP* Lubricomp* LEXAN_LF0335 compound is a 35% glass fiber, milled glass reinforced PC injection moulding resin with improved wear resistance and reduced friction.
Melt Index of Compound 9.0 g/10 min

@Load 5.00 kg,
Temperature 250 °C
9.0 g/10 min

@Load 11.0 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Europe-Africa-Middle East)
Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin.
Melt Index of Compound 9.0 - 16 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.0 - 16 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Spec
Axion Polymers Axpoly® PP06 5001 Enhanced Black General Purpose Polypropylene
PP06 Series polypropylene offer the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PP06 range of resin co..
Melt Index of Compound 9.0 g/10 min

@Load 2.16 kg,
Temperature 250 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® 315 PBT (Europe-Africa-Middle East)
VALOX 315 is compliant with food contact regulations acc. to EC Reg. No. 10/2011. VALOX 315 can be applied for injection moulding and extrusion puposes.