Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 29 g/10 min @Load 5.00 kg, Temperature 260 °C |
29 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics GELOY HRA170D ASA+PC (Europe-Africa-Middle East) GELOY HRA170D resin is a PC-ASA blend with permanent antistatic behavior. It is typically used in applications that require antidust properties and high impact retention. Geloy HRA170D resin is typi.. |