Physical Properties Metric English Comments
Melt Index of Compound 22 g/10 min

@Load 5.00 kg,
Temperature 260 °C
22 g/10 min

@Load 11.0 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Cycoloy® FXC630ME PC+ABS
Color package may affect performance. PC+ABS, ECO-conforming flame retardant with metallic or pearlescent appearance.
Melt Index of Compound 22 g/10 min

@Load 5.00 kg,
Temperature 260 °C
22 g/10 min

@Load 11.0 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Cycoloy® FXC630ME PC+ABS (Asia Pacific)
PC+ABS, ECO-conforming flame retardant with metallic or pearlescent appearance.
Melt Index of Compound 22 g/10 min

@Load 5.00 kg,
Temperature 260 °C
22 g/10 min

@Load 11.0 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS
High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).
Melt Index of Compound 22 g/10 min

@Load 5.00 kg,
Temperature 260 °C
22 g/10 min

@Load 11.0 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Asia Pacific)
High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).
Melt Index of Compound 22 g/10 min

@Load 5.00 kg,
Temperature 260 °C
22 g/10 min

@Load 11.0 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Europe-Africa-Middle East)
High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).
Melt Index of Compound 22 g/10 min

@Load 5.00 kg,
Temperature 260 °C
22 g/10 min

@Load 11.0 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Cycoloy® C1200HF PC+ABS (Europe-Africa-Middle East)
CYCOLOY C1200HF is the improved version of CYCOLOY C1200 and has been developed to provide enhanced productivity and surface appearance for
Melt Index of Compound 22 g/10 min

@Load 2.16 kg,
Temperature 330 °C
22 g/10 min

@Load 4.76 lb,
Temperature 626 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics LNP LUBRICOMP DX09410H PC
LNP* LUBRICOMP* DX09410H is a compound based on Polycarbonate resin containing Proprietary FIllers. Added features of this grade include: Healthcare, Wear Resistant.
Melt Index of Compound 22 g/10 min

@Load 5.00 kg,
Temperature 265 °C
22 g/10 min

@Load 11.0 lb,
Temperature 509 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® 359 PBT (Europe-Africa-Middle East)
VALOX 359 is an unreinforced, flame retarded, low warpage PBT injection moulding resin.
Melt Index of Compound 22 g/10 min

@Load 5.00 kg,
Temperature 250 °C
22 g/10 min

@Load 11.0 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® 815F PBT+PET (Europe-Africa-Middle East)
PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications
Melt Index of Compound 22 g/10 min

@Load 5.00 kg,
Temperature 250 °C
22 g/10 min

@Load 11.0 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® DR48V PBT (Europe-Africa-Middle East)
VALOX DR48V is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot..
Melt Index of Compound 22 g/10 min

@Load 5.00 kg,
Temperature 260 °C
22 g/10 min

@Load 11.0 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL PVX0800 PPE
NORYL* PVX0800 resin is a high flow, V0 = 1.5 mm grade, suitable for a variety of electronics applications.
Melt Index of Compound 22 g/10 min

@Load 2.16 kg,
Temperature 280 °C
22 g/10 min

@Load 4.76 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS
Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen..
Melt Index of Compound 22 g/10 min

@Load 2.16 kg,
Temperature 280 °C
22 g/10 min

@Load 4.76 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS (Asia Pacific)
Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen..
Melt Index of Compound 22 g/10 min

@Load 2.16 kg,
Temperature 280 °C
22 g/10 min

@Load 4.76 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS (Europe-Africa-Middle East)
Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen..