Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 18 g/10 min @Load 5.00 kg, Temperature 260 °C |
18 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics GELOY XP4025 ASA (Europe-Africa-Middle East) GELOY XP4025 is a high heat modified ASA/PC blend, for automotive exterior applications. It shows very good properties, gloss and colour retention, as well as faster cycle time over competitive mate.. |
|||
Melt Index of Compound | 18 g/10 min @Load 2.16 kg, Temperature 280 °C |
18 g/10 min @Load 4.76 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL V090 PPE+HIPS (Europe-Africa-Middle East) NORYL V090 is an unfilled, flame retardant material with a Vicat B/120 of 95 °C according ISO 306. NORYL V090 is V0 at 2.0 mm and V1 at 1.6 mm according UL94 and halogen free according VDE/DIN 47.. |
|||
Melt Index of Compound | 18 g/10 min @Load 2.16 kg, Temperature 250 °C |
18 g/10 min @Load 4.76 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® 4012 PBT (Europe-Africa-Middle East) VALOX 4012 is a 10% high strength glass fibre reinforced PBT injection moulding resin with improved mechanical properties. Applications: connectors. |
|||
Melt Index of Compound | 18 g/10 min @Load 5.00 kg, Temperature 250 °C |
18 g/10 min @Load 11.0 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® ENH4530 PBT (Europe-Africa-Middle East) 15% GF PBT, Non-Brominated & Non-Chlorinated Flame retardant |
|||
Melt Index of Compound | 18 g/10 min @Load 5.00 kg, Temperature 250 °C |
18 g/10 min @Load 11.0 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® ENH4565 PBT (Asia Pacific) 33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE. |
|||
Melt Index of Compound | 18 g/10 min @Load 5.00 kg, Temperature 250 °C |
18 g/10 min @Load 11.0 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® ENH4565 PBT (Europe-Africa-Middle East) 33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE. |
|||
Melt Index of Compound | 18 g/10 min @Load 2.16 kg, Temperature 250 °C |
18 g/10 min @Load 4.76 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® VX5011 PBT (Europe-Africa-Middle East) VALOX VX5011 is a 10% glass fibre reinforced PBT+PC blend with low warpage characteristics. |
|||
Melt Index of Compound | 18 g/10 min @Load 5.00 kg, Temperature 265 °C |
18 g/10 min @Load 11.0 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Melt Index of Compound | 18 g/10 min @Load 5.00 kg, Temperature 265 °C |
18 g/10 min @Load 11.0 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Asia Pacific) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Melt Index of Compound | 18 g/10 min @Load 5.00 kg, Temperature 265 °C |
18 g/10 min @Load 11.0 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Melt Index of Compound | 18 g/10 min @Load 5.00 kg, Temperature 250 °C |
18 g/10 min @Load 11.0 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® EXVX1403 PBT (Asia Pacific) 33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE. |
|||
Melt Index of Compound | 18 g/10 min @Load 5.00 kg, Temperature 250 °C |
18 g/10 min @Load 11.0 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® IQNH4565 PBT (Asia Pacific) Valox* iQNH4565 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 29% based on EPEAT.. |
|||
Melt Index of Compound | 18 g/10 min @Load 2.16 kg, Temperature 265 °C |
18 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics XYLEX EXXX0292 PC+POLYESTER (Europe-Africa-Middle East) XYLEX* EXXX0292 is a transparent copolyester/polycarbonate blend with high flow, V2 UL94 rating at 1.5mm and Tg of 108 C |