Physical Properties Metric English Comments
Melt Index of Compound 15 g/10 min

@Load 3.80 kg,
Temperature 280 °C
15 g/10 min

@Load 8.38 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL V03505 PPE+HIPS
Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Melt Index of Compound 15 g/10 min

@Load 3.80 kg,
Temperature 280 °C
15 g/10 min

@Load 8.38 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Asia Pacific)
Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Melt Index of Compound 15 g/10 min

@Load 3.80 kg,
Temperature 280 °C
15 g/10 min

@Load 8.38 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Europe-Africa-Middle East)
Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Melt Index of Compound 15 g/10 min

@Load 5.00 kg,
Temperature 250 °C
15 g/10 min

@Load 11.0 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® 310SE0 PBT (Europe-Africa-Middle East)
VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings.
Melt Index of Compound 15 g/10 min

@Load 5.00 kg,
Temperature 250 °C
15 g/10 min

@Load 11.0 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® 5031 PBT (Europe-Africa-Middle East)
VALOX 5031 is a 30% glass reinforced PBT+PC blend with low warpage characteristics. Applications: appliance handles, automotive doorhandles. This grade is a 508 with reduced warpage.
Melt Index of Compound 15 g/10 min

@Load 2.16 kg,
Temperature 265 °C
15 g/10 min

@Load 4.76 lb,
Temperature 509 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Europe-Africa-Middle East)
VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin..
Melt Index of Compound 15 g/10 min

@Load 2.16 kg,
Temperature 265 °C
15 g/10 min

@Load 4.76 lb,
Temperature 509 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® 865 PBT (Europe-Africa-Middle East)
VALOX 865 is a 30% glass fibre reinforced, non blooming flame retardant PBT+PET blend with an excellent surface appearance. Applications: External housings, steam irons, appliance housings and light..
Melt Index of Compound 15 g/10 min

@Load 2.16 kg,
Temperature 250 °C
15 g/10 min

@Load 4.76 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® DR51 PBT (Europe-Africa-Middle East)
VALOX DR51 is a 15% glass fiber reinforced PBT injection moulding resin with excellent mechanical, thermal and electrical performance. Applications: spotlights, appliance housings, handles.
Melt Index of Compound 15 g/10 min

@Load 5.00 kg,
Temperature 265 °C
15 g/10 min

@Load 11.0 lb,
Temperature 509 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East)
Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified.
Melt Index of Compound 15 g/10 min

@Load 5.00 kg,
Temperature 250 °C
15 g/10 min

@Load 11.0 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ASTM D1238
SABIC Innovative Plastics Xenoy® 5220U PBT+PC (Asia Pacific)
Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance.
Melt Index of Compound 15 g/10 min

@Load 5.00 kg,
Temperature 250 °C
15 g/10 min

@Load 11.0 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Xenoy® 5220U PBT+PC (Asia Pacific)
Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance.
Melt Index of Compound 15 g/10 min

@Load 1.20 kg,
Temperature 280 °C
15 g/10 min

@Load 2.65 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Asia Pacific)
Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a..
Melt Index of Compound 15 g/10 min

@Load 5.00 kg,
Temperature 230 °C
15 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
3M Dyneon™ PVDF 31508/0003 Polyvinylidene Fluoride
3M™ Dyneon™ PVDF 31508/0003 is a flexible copolymer of VF2 and CTFE, exhibiting very low shrinkage and excellent impact resistance. PVDF 31508/0003 also has a very low brittleness temperature, for..
Melt Index of Compound 15 g/10 min

@Load 5.00 kg,
Temperature 230 °C
15 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
3M Dyneon™ PVDF 32008/0009 Polyvinylidene Fluoride
3M™ Dyneon™ PVDF 32008/0009 is an ultra-flexible copolymer of VF2 and CTFE, exhibiting very low shrinkage and excellent impact resistance. Dyneon PVDF 32008/0009 also has a very low brittleness te..
Melt Index of Compound 15 g/10 min

@Load 5.00 kg,
Temperature 230 °C
15 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
3M Dyneon™ PVDF 31508/0001 Polyvinylidene Fluoride  (discontinued **)
Copolymer of VF2 and CTFEUltra-flexibleVery low shrinkage ratesWide operating temperature windowProcessable using a variety of thermoplastic conversation techniquesInformation provided by Dyneon, A ..
Melt Index of Compound 15 g/10 min

@Load 5.00 kg,
Temperature 230 °C
15 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
3M Dyneon™ PVDF 32008/0003 Polyvinylidene Fluoride  (discontinued **)
Copolymer of VF2 and CTFEUltra-flexibleVery low shrinkage ratesWide operating temperature windowProcessable using a variety of thermoplastic conversion techniquesExcellent low flame and low smoke pe..
Melt Index of Compound 15 g/10 min

@Load 5.00 kg,
Temperature 230 °C
15 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
3M Dyneon™ PVDF 31508/0009 Polyvinylidene Fluoride
3M™ Dyneon™ PVDF 31508/0009 is a flexible copolymer of VF2 and CTFE, exhibiting very low shrinkage and excellent impact resistance. Dyneon PVDF 31508/0009 also has a very low brittleness temperatu..
Melt Index of Compound 15 g/10 min

@Load 1.20 kg,
Temperature 280 °C
15 g/10 min

@Load 2.65 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL FP6130 PPE+PS
Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a..
Melt Index of Compound 15 g/10 min

@Load 1.20 kg,
Temperature 280 °C
15 g/10 min

@Load 2.65 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Europe-Africa-Middle East)
Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a..
Melt Index of Compound 15 g/10 min

@Load 5.00 kg,
Temperature 230 °C
15 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
3M Dyneon™ PVDF 31008/0003 Polyvinylidene Fluoride  (discontinued **)
3M™ Dyneon™ PVDF 31008/0003 is a flexible copolymer of VF2 and CTFE, exhibiting very low shrinkage and excellent impact resistance. Dyneon PVDF 31008/0003 also has a very low brittleness temperatu..
Melt Index of Compound 15 g/10 min

@Load 5.00 kg,
Temperature 230 °C
15 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
3M Dyneon™ PVDF 31008/0009 Polyvinylidene Fluoride  (discontinued **)
Copolymer of VF2 and CTFEUltra-flexibleVery low shrinkage ratesWide operating temperature windowProcessable using a variety of thermoplastic conversation techniquesExcellent low flame and low smoke ..
Melt Index of Compound 15 g/10 min

@Load 5.00 kg,
Temperature 230 °C
15 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
3M Dyneon™ PVDF 32008/0000 Polyvinylidene Fluoride  (discontinued **)
Copolymer of VF2 and CTFEUltra-flexibleVery low shrinkage ratesWide operating temperature windowProcessable using a variety of thermoplastic conversion techniquesInformation provided by Dyneon, A 3M..