Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Index of Compound = 10 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Index of Compound 10 g/10 min

@Load 5.00 kg,
Temperature 220 °C
10 g/10 min

@Load 11.0 lb,
Temperature 428 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Cycolac® FXS600AR ABS (Europe-Africa-Middle East)
Visual Ares effect Cycolac ABS material with excellent flow properties.
Melt Index of Compound 10 g/10 min

@Load 5.00 kg,
Temperature 260 °C
10 g/10 min

@Load 11.0 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Cycoloy® XCM840 PC+ABS
High stiffness PC/ABS blend offering practical impact, low CTE, high heat resistance, with good aesthetics suitable for injection molding
Melt Index of Compound 10 g/10 min

@Load 5.00 kg,
Temperature 260 °C
10 g/10 min

@Load 11.0 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics GELOY CR8510 ASA
ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated.
Melt Index of Compound 10 g/10 min

@Load 5.00 kg,
Temperature 260 °C
10 g/10 min

@Load 11.0 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics GELOY CR8510 ASA (Asia Pacific)
ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated.
Melt Index of Compound 10 g/10 min

@Load 5.00 kg,
Temperature 260 °C
10 g/10 min

@Load 11.0 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics GELOY CR7500 ASA (Europe-Africa-Middle East)
High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only.
Melt Index of Compound 10 g/10 min

@Load 2.16 kg,
Temperature 260 °C
10 g/10 min

@Load 4.76 lb,
Temperature 500 °F
Honeywell Aegis™ OX High Barrier Nylon  (discontinued **)
Description: Aegis OX is an oxygen-scavenging nylon. Oxygen barrier is comparable to a glass bottle with metal crown closure. In addition Aegis OX provides CO2 barrier and possesses glass-like cla..
Melt Index of Compound 10 g/10 min

@Load 5.00 kg,
Temperature 280 °C
10 g/10 min

@Load 11.0 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL PX9406P PPE+HIPS (Asia Pacific)
Nonbrominated, nonchlorinated, flame retarded. Improved productivity and reliability. 125dc HDT. UL94 V-0 rated. Electrical applications.
Melt Index of Compound 10 g/10 min

@Load 5.00 kg,
Temperature 300 °C
10 g/10 min

@Load 11.0 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL V01550 PPE+HIPS (Europe-Africa-Middle East)
NORYL V01550 is a 15 % short glass fibre reinforced, flame retardant material with a HDT/A of 130C according ISO 75. NORYL V01550 is V0 at 0.75 mm according UL94 and is halogen free according VDE/DI..
Melt Index of Compound 10 g/10 min

@Load 1.20 kg,
Temperature 280 °C
10 g/10 min

@Load 2.65 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL V090 PPE+HIPS (Europe-Africa-Middle East)
NORYL V090 is an unfilled, flame retardant material with a Vicat B/120 of 95 °C according ISO 306. NORYL V090 is V0 at 2.0 mm and V1 at 1.6 mm according UL94 and halogen free according VDE/DIN 47..
Melt Index of Compound 10 g/10 min

@Load 5.00 kg,
Temperature 265 °C
10 g/10 min

@Load 11.0 lb,
Temperature 509 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® 357X PBT (Europe-Africa-Middle East)
VALOX 357X is an impact modified, flame retarted PBT+PC blend. Applications like bobbins, switches and enclosures.
Melt Index of Compound 10 g/10 min

@Load 5.00 kg,
Temperature 250 °C
10 g/10 min

@Load 11.0 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ASTM D1238
SABIC Innovative Plastics Valox® ENH8560 PBT+PET (Europe-Africa-Middle East)
Non-Brominated & Non-Chlorinated Flame Retardant, 30% Glass fiber reinforced PBT/PET blend
Melt Index of Compound 10 g/10 min

@Load 5.00 kg,
Temperature 250 °C
10 g/10 min

@Load 11.0 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Xenoy® 5720U PBT+PC
Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY
Melt Index of Compound 10 g/10 min

@Load 5.00 kg,
Temperature 250 °C
10 g/10 min

@Load 11.0 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Asia Pacific)
Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY
Melt Index of Compound 10 g/10 min

@Load 5.00 kg,
Temperature 250 °C
10 g/10 min

@Load 11.0 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East)
Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY
Melt Index of Compound 10 g/10 min

@Load 2.16 kg,
Temperature 265 °C
10 g/10 min

@Load 4.76 lb,
Temperature 509 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER
PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility
Melt Index of Compound 10 g/10 min

@Load 2.16 kg,
Temperature 265 °C
10 g/10 min

@Load 4.76 lb,
Temperature 509 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER (Asia Pacific)
PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility
Melt Index of Compound 10 g/10 min

@Load 2.16 kg,
Temperature 265 °C
10 g/10 min

@Load 4.76 lb,
Temperature 509 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER (Europe-Africa-Middle East)
PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility
Melt Index of Compound 10 g/10 min

@Load 10.0 kg,
Temperature 220 °C
10 g/10 min

@Load 22.0 lb,
Temperature 428 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Cycolac® DL100LG ABS (Europe-Africa-Middle East)
Cycolac DL100LG is a low gloss, high heat, high impact ABS/PC blend with low emission
Melt Index of Compound 10 g/10 min

@Load 5.00 kg,
Temperature 260 °C
10 g/10 min

@Load 11.0 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics GELOY CR7500 ASA (Asia Pacific)
High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only.
Melt Index of Compound 10 g/10 min

@Load 5.00 kg,
Temperature 260 °C
10 g/10 min

@Load 11.0 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics GELOY CR7500 ASA
High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only.
Copyright © lookpolymers.com All Rights Reserved