Physical Properties | Metric | English | Comments |
---|---|---|---|
Carbon Dioxide Transmission | 380 - 429 cc-mm/m²-24hr-atm | 965 - 1090 cc-mil/100 in²-24hr-atm | Average value: 405 cc-mm/m²-24hr-atm Grade Count:4 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Carbon Dioxide Transmission | 380 - 429 cc-mm/m²-24hr-atm | 965 - 1090 cc-mil/100 in²-24hr-atm | Average value: 405 cc-mm/m²-24hr-atm Grade Count:3 |
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Carbon Dioxide Transmission | 380 - 480 cc-mm/m²-24hr-atm | 965 - 1220 cc-mil/100 in²-24hr-atm | Average value: 417 cc-mm/m²-24hr-atm Grade Count:12 |
Overview of materials for Polycarbonate, UV Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a.. |
|||
Carbon Dioxide Transmission | 380 cc-mm/m²-24hr-atm @Thickness 0.100 mm |
965 cc-mil/100 in²-24hr-atm @Thickness 0.00394 in |
3800 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® LED2643 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• LED lighting, optics, .. |
|||
Carbon Dioxide Transmission | 380 - 480 cc-mm/m²-24hr-atm | 965 - 1220 cc-mil/100 in²-24hr-atm | Average value: 429 cc-mm/m²-24hr-atm Grade Count:20 |
Overview of materials for Polycarbonate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri.. |