Physical Properties | Metric | English | Comments |
---|---|---|---|
Carbon Dioxide Transmission | 76.0 cc-mm/m²-24hr-atm | 193 cc-mil/100 in²-24hr-atm | ASTM D1434 |
NatureWorks® Ingeo™ 4032D Film Grade PLA NatureWorks® PLA (polylactide) polymer 4032D can be converted into a biaxially oriented film with use temperatures up to 300°F (150°C). This film has excellent optics, good machinability and exce.. |