Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 0.550 cc-mm/m²-24hr-atm | 1.40 cc-mil/100 in²-24hr-atm | at 14.2 lbs/ream coating (1.0 mil); ASTM E96-53T |
Chevron Phillips MarFlex® 1013 LDPE Extrusion Coating Resin Resin Type: High Speed ResinCharacteristics: Excellent Processability, High Temperature Extrusion Stability, Good Draw Down ResinApplications: Food Packaging, LaminationsData provided by Chevron Che.. |
|||
Moisture Vapor Transmission | 0.550 cc-mm/m²-24hr-atm | 1.40 cc-mil/100 in²-24hr-atm | at 14.2 lbs/ream coating (1.0 mil); ASTM E96-53T |
Chevron Phillips MarFlex® 1019 Extrusion Coating Resin Resin Type: Very High Speed at Low Coating WeightsCharacteristics: Excellent Processability, Process at Lower Temperature, High Temperature Stability, Excellent Draw Down ResinApplications:Food Pack.. |