Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 0.260 cc-mm/m²-24hr-atm | 0.660 cc-mil/100 in²-24hr-atm | ASTM F1249 |
Chevron Phillips mPact™ D449 HDPE Blown Film Resin
(discontinued **) Resin Type: High density, hexene copolymerCharacteristics: excellent clarity, high gloss, good modulus, process with LLDPE setup, optimum clarity when used as an individual layer.Applications: overw.. |
|||
Moisture Vapor Transmission | 0.260 cc-mm/m²-24hr-atm | 0.660 cc-mil/100 in²-24hr-atm | ASTM E96 Procedure E |
DuPont™ Sclairfilm® LWS-1 LMDPE Film, Laminating, 50.8 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.LWS is a linear medium density polyolefin film produced from Sclair® copolymer resin and designed primarily for laminating end uses. It is treated on one.. |
|||
Moisture Vapor Transmission | 0.260 cc-mm/m²-24hr-atm | 0.660 cc-mil/100 in²-24hr-atm | ASTM E96 Procedure E |
DuPont™ Sclairfilm® LWS-2 LMDPE Film, Laminating, 50.8 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.LWS is a linear medium density polyolefin film produced from Sclair® copolymer resin and designed primarily for laminating end uses. It is treated on one.. |