Physical Properties Metric English Comments
Moisture Vapor Transmission 0.170 cc-mm/m²-24hr-atm
0.432 cc-mil/100 in²-24hr-atm
ASTM F1249
Chevron Phillips HiD® 9605D HDPE Cast Film Resin  (discontinued **)
Characteristics: Very Low Gel Levels, Produces Very "Clear" Film, Draws to Thin Gauges, Low Taste and Odor Transfer, Excellent MVTR for a Chill Cast Film, Excellent Processability, Excellent Optical..
Moisture Vapor Transmission 0.170 cc-mm/m²-24hr-atm
0.432 cc-mil/100 in²-24hr-atm
ASTM F1249
Chevron Phillips HiD® 9607D HDPE Cast Film Resin  (discontinued **)
Characteristics: Very Low Gel Levels, Produces Very "Clear" Film, Draws to Thin Gauges, Low Taste and Odor Transfer, Excellent MVTR for a Chill Cast Film, Excellent Processability, Excellent Optical..
Moisture Vapor Transmission 0.170 cc-mm/m²-24hr-atm
0.432 cc-mil/100 in²-24hr-atm
ASTM F1249
Chevron Phillips MarFlex® 9607XD HDPE Cast Film Resin  (discontinued **)
Characteristics: Very Low Gel Levels, Produces Very "Clear" Film, Draws to Thin Gauges, Low Taste and Odor Transfer, Excellent MVTR for a Chill Cast Film, Excellent Processability, Excellent Optical..
Moisture Vapor Transmission 0.170 cc-mm/m²-24hr-atm
0.432 cc-mil/100 in²-24hr-atm
ASTM F1249
Chevron Phillips MarFlex® 9607 HDPE Cast Film Resin
Characteristics: Very Low Gel Levels, Produces Very "Clear" Film, Draws to Thin Gauges, Low Taste and Odor Transfer, Excellent MVTR for a Chill Cast Film, Excellent Processability, Excellent Optical..
Moisture Vapor Transmission 0.170 cc-mm/m²-24hr-atm
0.432 cc-mil/100 in²-24hr-atm
ASTM E96 Procedure E
DuPont Teijin Films Mylar® M30 Polyester Film, 75 Gauge (21 µm), PVDC Coated  (discontinued **)
Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on both sides with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and..