Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 0.0900 cc-mm/m²-24hr-atm | 0.229 cc-mil/100 in²-24hr-atm | ASTM E96 Procedure E |
DuPont Teijin Films Mylar® M45 Polyester Film, 50 Gauge (15 µm), PVDC Coated
(discontinued **) Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, dispersion coated on one side with a PVDC copolymer. The coating is an excellent moisture and oxygen barrier. M45.. |
|||
Moisture Vapor Transmission | 0.0900 - 0.110 cc-mm/m²-24hr-atm | 0.229 - 0.279 cc-mil/100 in²-24hr-atm | Average value: 0.0922 cc-mm/m²-24hr-atm Grade Count:9 |
Overview of materials for Cyclo Olefin Polymer This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Moisture Vapor Transmission | 0.0900 cc-mm/m²-24hr-atm | 0.229 cc-mil/100 in²-24hr-atm | 1 atm; ASTM D1249 |
Mitsui APELâ„¢ APL5014DP Cyclo Olefin Copolymer (COC) This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces.. |
|||
Moisture Vapor Transmission | 0.0900 cc-mm/m²-24hr-atm | 0.229 cc-mil/100 in²-24hr-atm | 1 atm; ASTM D1249 |
Mitsui APELâ„¢ APL6011T Cyclo Olefin Copolymer (COC) This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces.. |
|||
Moisture Vapor Transmission | 0.0900 cc-mm/m²-24hr-atm | 0.229 cc-mil/100 in²-24hr-atm | 1 atm; ASTM D1249 |
Mitsui APELâ„¢ APL6015T Cyclo Olefin Copolymer (COC) This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces.. |
|||
Moisture Vapor Transmission | 0.0900 cc-mm/m²-24hr-atm | 0.229 cc-mil/100 in²-24hr-atm | 1 atm; ASTM D1249 |
Mitsui APELâ„¢ APL8008T Cyclo Olefin Copolymer (COC) This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces.. |
|||
Moisture Vapor Transmission | 0.0900 cc-mm/m²-24hr-atm | 0.229 cc-mil/100 in²-24hr-atm | 1 atm; ASTM D1249 |
Mitsui APELâ„¢ APL6013T Cyclo Olefin Copolymer (COC) This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces.. |
|||
Moisture Vapor Transmission | 0.0900 cc-mm/m²-24hr-atm | 0.229 cc-mil/100 in²-24hr-atm | 1 atm; ASTM D1249 |
Mitsui APELâ„¢ APL6509T Cyclo Olefin Copolymer (COC) This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces.. |
|||
Moisture Vapor Transmission | 0.0900 cc-mm/m²-24hr-atm | 0.229 cc-mil/100 in²-24hr-atm | 40°C, 90%, 50-300μm; JIS K7129 |
Zeon Chemicals Zeonor® 1020R Cyclo Olefin Polymer Zeonor® is a line of thermoplastic polyolefin resin with an excellent combination of optical and electronic properties. These unique Cyclo Olefin Polymer (COP) was developed by Zeon Corporation usi.. |
|||
Moisture Vapor Transmission | 0.0900 cc-mm/m²-24hr-atm | 0.229 cc-mil/100 in²-24hr-atm | 40°C, 90%, 50-300μm; JIS K7129 |
Zeon Chemicals Zeonor® 1060R Cyclo Olefin Polymer Zeonor® is a line of thermoplastic polyolefin resin with an excellent combination of optical and electronic properties. These unique Cyclo Olefin Polymer (COP) was developed by Zeon Corporation usi.. |