Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 10% Igepal® | 220 hour @Temperature 50.0 °C |
220 hour @Temperature 122 °F |
F<sub>50</sub>; Condition A, From compression molded specimens; ASTM D1693 |
NOVA Chemicals Novapol® TR-0735-U Hexene MDPE Rotational Molding Resin Good impact resistance, Excellent processabilityApplications: Toys, Complex custom parts, Home and garden items, MailboxesAdditives: Processing antioxidants, UV stabilizersInformation provided by NO.. |
|||
ESCR 10% Igepal® | 220 hour | 220 hour | Condition A; ASTM D1693 |
NOVA Chemicals Novapol® TR-0735-UG Hexene MDPE Rotational Molding Resin Features: Good impact properties Excellent processabilityNSF listed for Stds. 14, 24 and 61 Applications: ToysComplex custom partsHome and garden itemsMailboxesInformation provided by Nova Chemicals.. |