Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 10% Igepal® | 190 hour | 190 hour | F50; ASTM D1693B |
ExxonMobil LLDPE LL 8450.31 Linear Low Density Polyethylene Resin Product Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that require.. |
|||
ESCR 10% Igepal® | 190 hour | 190 hour | F50; ASTM D1693B |
ExxonMobil LLDPE LLP 8450.31 Linear Low Density Polyethylene Resin Product Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that require.. |