Polymer Property : ESCR 10% Igepal® = 185 hour Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
ESCR 10% Igepal® 185 hour
185 hour
ASTM D1693
ExxonMobil LL 8450 Rotational Molding Resin  (discontinued **)
LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. This resin is ideally suited for applications that require optimum balance..
ESCR 10% Igepal® 185 hour
185 hour
ASTM D1693
ExxonMobil LL 8450.31 Rotational Molding Resin
Product Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that require..
ESCR 10% Igepal® 185 hour
185 hour
ASTM D1693
ExxonMobil LLP8450.31 Rotational Molding Resin
LProduct Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that requir..
ESCR 10% Igepal® 185 hour

@Temperature 50.0 °C
185 hour

@Temperature 122 °F
h/F50; Compression molded 2mm notched-plaques; ASTM D1693
Braskem Green PE SGM7746C Blow Molding and Monofilament High Density Polyethylene
Lower greenhouse gas emissions100% made from renewable raw materialsPerformance and Competitiveness: Green Polyethylene has the same characteristics as petrochemical polyethyleneApplications: Mono..