Polymer Property : ESCR 10% Igepal® = 16 hour Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
ESCR 10% Igepal® 16 hour
16 hour
F50; ASTM D1693B
SABIC BM6246LS High Density Polyethylene for Blow Molding
Product Description: BM6246LS grade is a medium molecular weight High Density Polyethylene homopolymer for blow molding applications. It is primarily designed for imparting high rigidity, toughnes..
ESCR 10% Igepal® 16 hour

@Thickness 2.00 mm,
Temperature 50.0 °C
16 hour

@Thickness 0.0787 in,
Temperature 122 °F
0.3 mm notched-plaques; ASTM-D1693
Braskem GD5160 HDPE Blow Molding Polyethylene Homopolymer
GD5160 is a high-density polyethylene homopolymer with high density and stiffness combined with high impact resistance and productivity. It was developed for the blow-molding segment. It is used in ..