Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 100% Igepal® | 24 hour | 24 hour | F50; ASTM D1693B |
SABIC BM6246LS High Density Polyethylene for Blow Molding Product Description: BM6246LS grade is a medium molecular weight High Density Polyethylene homopolymer for blow molding applications. It is primarily designed for imparting high rigidity, toughnes.. |
|||
ESCR 100% Igepal® | 24 hour @Thickness 3.00 mm, Temperature 23.0 °C |
24 hour @Thickness 0.118 in, Temperature 73.4 °F |
compression molded plaques; ASTM D1693B |
Braskem HM 150 HDPE Monofilament Polyethylene
(discontinued **) Applications: Raschel; flat yarn; general and industrial rape netting. Information provided by Braskem |
|||
ESCR 100% Igepal® | 24 hour | 24 hour | Condition B, F50; ASTM D1693 |
Chevron Phillips Marlex® 9519H High Density Polyethylene, Blow Molding This gas phase, high molecular weight, homopolymer with antistatic agent is tailored for lightweight blow molded applications that:Require excellent stiffness to ESCR ratioRequire good melt strength.. |
|||
ESCR 100% Igepal® | 24 hour | 24 hour | Condition B, F50; ASTM D1693 |
Chevron Phillips Marlex® 9518H High Density Polyethylene, Blow Molding This gas phase, high molecular weight, homopolymer is tailored for lightweight blow molded applications that:Require excellent stiffness to ESCR ratioRequire good melt strengthAre durable and recycl.. |