Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 100% Igepal® | 11 hour @Temperature 50.0 °C |
11 hour @Temperature 122 °F |
ASTM D1693 |
Unipetrol PE HD LITEN® VB 33 HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |