Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 92 cm³/g | 92 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
Lanxess Pocan® T 7323 000000 PBT + PET, 20% Glass Fiber PBT+PET, 20% glass fibers, injection molding, improved surface finish, increased temperature peak load |
|||
Viscosity Test | 92 cm³/g | 92 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
Lanxess Pocan® T 7323 POS151 000000 PBT + PET, 20% Glass Fiber PBT+PET, 20% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV-stabilized |
|||
Viscosity Test | 92 cm³/g | 92 cm³/g | Reduced viscosity, K value = 61; ISO 1628-2 |
SolVin 561SF Vinyl Chloride - Vinyl Acetate copolymer Paste - filler Made by suspension polymerization.
APPLICATIONS
This resin has been especially developed for automotive mastics.Information provided by SolVin. |
|||
Viscosity Test | 92 cm³/g | 92 cm³/g | Viscosity number |
BASF Ultradur B 2300 G6 HR BK15116 30% Glass Filled PBT Ultradur B 2300 G6 HR BK15116 is a hydrolysis resistant, pigmented black 30% fiberglass reinforced PBT, exhibiting superior flow characteristics. Designed for improved latch
strength in automotive.. |