Polymer Property : Viscosity Test = 91 cm³/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity Test 91 cm³/g
91 cm³/g
Viscosity number; ISO 307, 1157, 1628
Lanxess Pocan® T 7331 POS151 000000 PBT + PET, 30% Glass Fiber  (discontinued **)
PBT+PET, 30% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV-stabilized
Viscosity Test 91 cm³/g
91 cm³/g
Viscosity number; ISO 307, 1157, 1628
Lanxess Pocan® T 7331 000000 PBT + PET, 30% Glass Fiber
PBT+PET, 30% glass fibers, injection molding, improved surface finish, increased temperature peak load
Viscosity Test 91 cm³/g
91 cm³/g
Viscosity number; ISO 1628-5
Lanxess Pocan® T 7331 POS151 700226 PBT + PET, 30% Glass Fiber
PBT + PET, 30% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV stabilizedInformation provided by LANXESS.