Physical Properties Metric English Comments
Viscosity Test 80 cm³/g
80 cm³/g
Viscosity number; ISO 307, 1157, 1628
Lanxess Pocan® T 7391 POS151 000000 PBT + PET, 45% Glass Fiber  (discontinued **)
PBT+PET, 45% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV-stabilized
Viscosity Test 80 cm³/g
80 cm³/g
Viscosity number; ISO 307, 1157, 1628
Lanxess Pocan® T 7391 000000 PBT + PET, 45% Glass Fiber
PBT+PET, 45% glass fibers, injection molding, improved surface finish, increased temperature peak load
Viscosity Test 80 cm³/g
80 cm³/g
Viscosity number; ISO 1628-5
Lanxess Pocan® T 7391 POS151 900044 PBT + PET, 45% Glass Fiber
PBT + PET, 45% glass fibers, injection molding, improved surface finish, increased temperature peak load UV stabilizedInformation provided by LANXESS.
Viscosity Test 80 - 84 cm³/g
80 - 84 cm³/g
Ubbelhode
Iran Petrochemical (PCC) PET BG-825 Polyethylene Terephthalate
Polyethylene Terephthalate, bottle gradeApplications: CSD, carbonated water, edible oil, alcoholic beverage, pharmaceuticals, wild mouth jars, APET sheet, strappingInformation provided by Iran Petro..
Viscosity Test 80 cm³/g
80 cm³/g
Viscosity number; ISO 307, 1157, 1628
Lanxess Pocan® C 3230 XF 000000 PBT + PC, 30% Glass Fiber
PBT+PC, 30% glass fibers, injection molding, improved flowability, low tendency to warp, improved surface finish
Viscosity Test 80 cm³/g
80 cm³/g
Reduced viscosity, K value = 57; ISO 1628-2
SolVin 257RF Polyvinyl Chloride General Purpose - Rigid
Made by suspension polymerization. APPLICATIONS Extrusion : unplasticized PVC - profile - foam - sheet, film - blow moldings Calendering : unplasticized PVC - film : high temperature process Injecti..
Viscosity Test 80 cm³/g
80 cm³/g
Reduced viscosity, K value = 57; ISO 1628-2
SolVin 258RD Polyvinyl Chloride General Purpose - Rigid
Made by suspension polymerization. APPLICATIONS Blow extrusion : opaque or crystal-clear bottles Injection molding : rigid articles Calendering : opaque or crystal-clear rigid sheets Extrusion : rig..
Viscosity Test 80 cm³/g
80 cm³/g
Reduced viscosity, K value = 57; ISO 1628-2
SolVin 557RA Copolymer of Vinyl Chloride and Vinyl Acetate
Made by suspension polymerization. APPLICATIONS Extrusion : sheets for vacuum-forming, for deformations of over 500 % Calendering : rigid sheets for deep thermoformingInformation provided by SolVin...
Viscosity Test 80 cm³/g
80 cm³/g
Reduced viscosity, K value = 57; ISO 1628-2
SolVin 557RB Copolymer of Vinyl Chloride and Vinyl Acetate
Made by suspension polymerization. APPLICATIONS Extrusion : sheets for vacuum-forming, for deformations of over 500 % Calendering : rigid sheets for deep thermoformingInformation provided by SolVin...
Viscosity Test 80 cm³/g
80 cm³/g
Viscosity Number
DSM Stanyl® 46HF5040 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Viscosity Test 80 cm³/g
80 cm³/g
DAM; ISO 307 1157 1628
DuPont Performance Polymers Zytel® 330 NC010 Nylon  (Unverified Data**)
Unreinforced PolyamideZytel 330 NC010 is a transparent polyamide resin with amorphous characteristics.Information provided by DuPont Performance Polymers
Viscosity Test 80 cm³/g
80 cm³/g
Viscosity number
BASF Ultradur B 4040 G6 High Speed BK15029 30% Glass Filled PBT/PET
Ultradur B 4040 G6 High Speed BK15029 is a high flow, fast cycling with low warpage, 30% glass filled, pigmented black, injection molding PBT for industrial parts, rigid tough and dimensional stable..
Viscosity Test 80 cm³/g
80 cm³/g
Viscosity Number
Arkema Group Lacovyl® RB 8010 PVC
LACOVYL RB 8010 is a low molecular weight vinyl chloride homopolymer produced by mass polymerization process using the Elf Atochem's latest technology.Its characteristics are : Viscosity index ..
Viscosity Test 80 cm³/g
80 cm³/g
Viscosity Number
Arkema Group Lacovyl® GA 7701 H Vinyl Copolymer
LACOVYL GA 7701 H is a copolymer of vinyl chloride and vinyl acetate produced by suspension polymerization process. It may be used by itself or blended with a PVC homopolymer of similar molecular we..
Viscosity Test 80 cm³/g
80 cm³/g
Viscosity Number
Arkema Group Lacovyl® GA 7701 Vinyl Copolymer
LACOVYL GA 7701 is a copolymer of vinyl chloride and vinyl acetate produced by suspension polymerization process. It may be used by itself or blended with a PVC homopolymer of similar molecular weig..