Polymer Property : Viscosity Test = 75 cm³/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity Test 75 cm³/g
75 cm³/g
90% HCOOH; ISO 307
Techmer ES HiFill® PA6 E2
Availability: North AmericaForms: PelletsProcessing Method: ExtrusionInformation provided by TP Composites, Inc.
Viscosity Test 75 cm³/g
75 cm³/g
Viscosity Number
DSM Stanyl® TW241F12 Nylon 46-60% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Viscosity Test 75 cm³/g
75 cm³/g
Viscosity number
BASF Ultradur B 4040 G10 High Speed BK15029 50% Glass Filled PBT/PET
Ultradur B 4040 G10 High Speed BK15029 is a high flow, fast cycling with low warpage, 50% glass filled, injection molding PBT for industrial parts, rigid tough and dimensional stable applications.
Viscosity Test 75 cm³/g
75 cm³/g
Viscosity number
BASF Ultradur B 4040 G10 LS High Speed BK15029 50% Glass Filled PBT/PET