Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 55 cm³/g | 55 cm³/g | Viscosity Number |
Mitsubishi Xantar® 22 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 55 cm³/g | 55 cm³/g | Viscosity Number |
Mitsubishi Xantar® 22 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 55 cm³/g | 55 cm³/g | Viscosity Number |
Mitsubishi Xantar® 22 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 55 cm³/g | 55 cm³/g | Viscosity Number |
Mitsubishi Xantar® F 22 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 55 cm³/g | 55 cm³/g | Viscosity Number |
Mitsubishi Xantar® FC 22 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 55 cm³/g | 55 cm³/g | Viscosity Number |
Mitsubishi Xantar® FC 22 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 55 cm³/g | 55 cm³/g | Limiting Viscosity Number; ISO 1628-4 |
Mitsubishi Xantar® SF 22 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 55 cm³/g | 55 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® FN727 NC010A Nylon 6
(Unverified Data**) Toughened Polyamide 6Information provided by DuPont Performance Polymers |
|||
Viscosity Test | 55 cm³/g | 55 cm³/g | Viscosity Number |
Mitsubishi Xantar® F 22 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher.. |