Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 50.0 - 120 cm³/g | 50.0 - 120 cm³/g | Average value: 81.6 cm³/g Grade Count:10 |
Overview of materials for Polyvinyl Chloride - Polyvinyl Acetate Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Chloride - Polyvinyl Acetate Copolymer". Each property range of values reported is minimum and.. |
|||
Viscosity Test | 50.0 - 95.0 cm³/g | 50.0 - 95.0 cm³/g | Average value: 80.9 cm³/g Grade Count:16 |
Overview of materials for PBT + PET Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of .. |