Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 245 cm³/g | 245 cm³/g | Viscosity Number; ISO 307, 1157, 1628 |
DSM Akulon® F136 PA6 Very High Viscosity, Film Extrusion |
|||
Viscosity Test | 245 cm³/g | 245 cm³/g | Viscosity Number; ISO 307, 1157, 1628 |
DSM Akulon® F136-C PA6 Film Extrusion, Very High Viscosity, Lubricated |
|||
Viscosity Test | 245 cm³/g | 245 cm³/g | Viscosity Number; ISO 307, 1157, 1628 |
DSM Akulon® F136-C1 PA6 Very High Viscosity, Film Extrusion, Lubricated |
|||
Viscosity Test | 245 cm³/g | 245 cm³/g | Viscosity Number |
DSM Akulon® F136-DH Nylon 6 (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Viscosity Test | 245 cm³/g | 245 cm³/g | Viscosity Number; ISO 307, 1157, 1628 |
DSM Akulon® F136-E1 PA6 Very High Viscosity, Lubricated, Nucleated, Film Extrusion |
|||
Viscosity Test | 245 cm³/g | 245 cm³/g | Viscosity Number; ISO 307, 1157, 1628 |
DSM Akulon® F136-E2 PA6 Very High Viscosity, Lubricated, Nucleated, Film Extrusion |
|||
Viscosity Test | 245 cm³/g | 245 cm³/g | Viscosity Number |
DSM Akulon® F136-E Nylon 6 (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |