Physical Properties Metric English Comments
Viscosity Test 134 cm³/g
134 cm³/g
Viscosity number; ISO 307, 1157, 1628
Lanxess Durethan® B 30 S 000000 Nylon 6
PA 6, injection molding-grade, non-reinforced, easy-flow, easy-release, rapid solidification
Viscosity Test 134 cm³/g
134 cm³/g
Viscosity number; ISO 307, 1157, 1628
Lanxess Durethan® BKV 115 H2.0 901510 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 15, even in..
Viscosity Test 134 cm³/g
134 cm³/g
Viscosity number; ISO 307, 1157, 1628
Lanxess Durethan® BKV 130 000000 Copolyamide, 30% Glass Fiber
CoPA, injection molding grade, 30% glass fibers, elastomer modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 30, even in..
Viscosity Test 134 cm³/g
134 cm³/g
Viscosity number; ISO 307, 1157, 1628
Lanxess Durethan® BKV 130 GIT 900116 Copolyamide, 30% Glass Fiber
CoPA, injection molding grade, 30% glass fibers, elastomer-modified, suitable for GIT (gas assisted technology), good surface finishApplication Examples: Chain-saw handles, office chair armrests, of..
Viscosity Test 134 cm³/g
134 cm³/g
Viscosity number; ISO 307, 1157, 1628
Lanxess Durethan® BKV 130 H2.0 901510 Copolyamide, 30% Glass Fiber
CoPA, injection molding grade, 30% glass fibers, elastomer-modified, electroplateable, improved notched impact strength and energy absorption under biaxial impact load, good heat-ageing resistance
Viscosity Test 134 cm³/g
134 cm³/g
Viscosity number; ISO 307, 1157, 1628
Lanxess Durethan® BKV 130 H3.0 101006 Copolyamide, 30% Glass Fiber
CoPA, injection molding grade, 30% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 30 H3.0, ev..
Viscosity Test 134 cm³/g
134 cm³/g
Viscosity number; ISO 307, 1157, 1628
Lanxess Durethan® BKV 140 000000 Copolyamide, 40% Glass Fiber
CoPA, injection molding grade, 40% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 40, even in..
Viscosity Test 134 cm³/g
134 cm³/g
Viscosity number; ISO 307, 1157, 1628
Lanxess Durethan® BKV 140 H2.0 900051 Copolyamide, 40% Glass Fiber
CoPA, injection molding grade, 40% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 40, even in..
Viscosity Test 134 cm³/g
134 cm³/g
Viscosity number; ISO 307, 1157, 1628
Lanxess Durethan® DP 1852/30 000000 Nylon 6, 30% Glass Fiber
PA 6, 30% glassfibers, UL V-0 at 0.75 mm (listed),GWIT:775°C at 0,75 mm, GWFI:960°C at 0.75 mm, CTI/A:400, good flowabilityApplication Examples: Hand-held barrel pump housings
Viscosity Test 134 cm³/g
134 cm³/g
Viscosity number; ISO 307, 1157, 1628
Lanxess Durethan® BKV 115 000000 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 15, even in..