Polymer Property : Viscosity Test = 1.5 cm³/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity Test 1.5 - 2.0 cm³/g
1.5 - 2.0 cm³/g
Intrinsic Viscosity; Metabolix STM-029
Metabolix Mirelâ„¢ I6003rp Biobased PHA Polymeric Modifier
I6003rp PHA enhances the processing and properties of recycled PVC. Offering excellent inherent miscibility in PVC to enable improved processing, I6003rp can lower torque and improve flow, while imp..