Polymer Property : Bead Size = 1.10 mm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bead Size 0.600 - 1.10 mm
0.0236 - 0.0433 in
SABIC EPS 550FF Expandable Polystyrene
Product Description: Fire retardant expanded Polystyrene EPS 550FF is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch proce..
Bead Size 0.600 - 1.10 mm
0.0236 - 0.0433 in
SABIC EPS 552 Expandable Polystyrene
Product Description: Standard expanded Polystyrene EPS 552 is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch process. EPS..