Physical Properties | Metric | English | Comments |
---|---|---|---|
Bead Size | 0.400 - 0.800 mm | 0.0157 - 0.0315 in | |
SABIC EPS 452 Expandable Polystyrene Product Description: Standard expanded Polystyrene EPS 452 is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch process. EPS.. |
|||
Bead Size | 0.200 - 0.800 mm | 0.00787 - 0.0315 in | Breda Laboratory Analytical Methods 90.30 |
NOVA Chemicals Dytherm® 170F Expandable Polystyrene This is a special flame retardant grade consisting of spherical beads of a blend of polystyrene and polyphenylene ether containing pentane as expansion agent, and a internal flame-retardant additive.. |
|||
Bead Size | 0.400 - 0.800 mm | 0.0157 - 0.0315 in | |
NOVA Chemicals Styrocell® B733A Expandable Polystyrene
(discontinued **) This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used as expansion agent, typically used as pre-expanded beads in the .. |
|||
Bead Size | 0.400 - 0.800 mm | 0.0157 - 0.0315 in | Breda Laboratory Analytical Methods 90.30 |
NOVA Chemicals Styrocell® B733A Expandable Polystyrene
(discontinued **) This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used as expansion agent, typically used as pre-expanded beads in the .. |
|||
Bead Size | 0.500 - 0.800 mm | 0.0197 - 0.0315 in | |
BASF Neopor® 2400 Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of flame-retardant silver-gray foams having a consider.. |
|||
Bead Size | 0.500 - 0.800 mm | 0.0197 - 0.0315 in | |
BASF Neopor® 2400 CT Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of flame-retardant silver-gray foams having a consider.. |
|||
Bead Size | 0.400 - 0.800 mm | 0.0157 - 0.0315 in | |
SABIC EPS 450FF Expandable Polystyrene Product Description: Fire retardant expanded Polystyrene EPS 450FF is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch proce.. |