Physical Properties | Metric | English | Comments |
---|---|---|---|
Bead Size | 0.400 - 0.900 mm | 0.0157 - 0.0354 in | |
IRPC Polimaxx Pentfoam 361F Expandable Polystyrene GENERAL: PENTFOAM "361F" IS A REGULAR GRADE (STANDARD GRADE) EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT. THIS GRADE IS DEVELOPED TO MEET THE DEMAND FOR FAST MOLDING CYCLES IN V.. |
|||
Bead Size | 0.700 - 0.900 mm | 0.0276 - 0.0354 in | |
BASF Styropor® P 326 M Expandable Polystyrene Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Molded parts with very good mechanical .. |
|||
Bead Size | 0.700 - 0.900 mm | 0.0276 - 0.0354 in | |
BASF Styropor® P 326 C Expandable Polystyrene Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Molded partsInformation provided by BAS.. |
|||
Bead Size | 0.700 - 0.900 mm | 0.0276 - 0.0354 in | |
BASF Styropor® P 326 Expandable Polystyrene Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Molded partsInformation provided by BAS.. |
|||
Bead Size | 0.400 - 0.900 mm | 0.0157 - 0.0354 in | |
IRPC Polimaxx Pentfoam 422F Expandable Polystyrene GENERAL: PENTFOAM "422F" IS A REGULAR GRADE (STANDARD GRADE) EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT. THIS GRADE IS DEVELOPED TO MEET THE DEMAND FOR FAST MOLDING CYCLES IN V.. |
|||
Bead Size | 0.400 - 0.900 mm | 0.0157 - 0.0354 in | |
IRPC Polimaxx Pentfoam 522F Expandable Polystyrene GENERAL: PENTFOAM "522F" IS A REGULAR GRADE (STANDARD GRADE) EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT. THIS GRADE IS DEVELOPED TO MEET THE DEMAND FOR FAST MOLDING CYCLES IN V.. |
|||
Bead Size | 0.400 - 0.900 mm | 0.0157 - 0.0354 in | |
IRPC Polimaxx Pentfoam 526W Expandable Polystyrene GENERAL: PENTFOAM "526W" IS A REGULAR GRADE (STANDARD GRADE) EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT.APPLICATIONS: PENTFOAM "526W" IS PARTICULARLY WELL SUITED FOR THE MANUFA.. |
|||
Bead Size | 0.400 - 0.900 mm | 0.0157 - 0.0354 in | |
IRPC Polimaxx Pentfoam 328H Expandable Polystyrene General: Pentfoam 328H is a high density grade expandable polystyrene containing pentane as blowing agent, this grade is developed to meet the demand for fast molding cycles in vacuum machineApplica.. |