Physical Properties | Metric | English | Comments |
---|---|---|---|
High Load Melt Index | 45 g/10 min @Load 21.6 kg, Temperature 200 °C |
45 g/10 min @Load 47.6 lb, Temperature 392 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PS 1326 PRE-ELEC PS 1326 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC .. |
|||
High Load Melt Index | 45 g/10 min @Load 21.6 kg, Temperature 190 °C |
45 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Braskem BT 003 HDPE Blow Molding Polyethylene
(discontinued **) Applications: Bottles for food products, lubricating and cooking oil; toys; bottler for surface-active agents; sheets. Information provided by Braskem |
|||
High Load Melt Index | 45 g/10 min @Load 21.6 kg, Temperature 190 °C |
45 g/10 min @Load 47.6 lb, Temperature 374 °F |
|
Meilian Chemical PE42089 YELLOW MASTERBATCH YELLOW PE42089 is a yellow LDPE-based masterbatch containing 30% Bisazo Benzidine yellow pigment, designed for use in polyolefin resins (PE and PP, etc.). Color Index No.:Yellow 83Method of Usage: Y.. |
|||
High Load Melt Index | 45 g/10 min @Load 21.6 kg, Temperature 190 °C |
45 g/10 min @Load 47.6 lb, Temperature 374 °F |
|
Meilian Chemical PE62072 RED MASTERBATCH RED 62072 is a red LDPE-based masterbatch containing 30% pigment, designed for use in polyolefin resins (PE and PP, etc..). Color Index No.: Red 57:1Method of Usage: RED PE62072 is designed for ease.. |
|||
High Load Melt Index | 45 g/10 min @Load 21.6 kg, Temperature 250 °C |
45 g/10 min @Load 47.6 lb, Temperature 482 °F |
|
BASF Luranyl® KR 2420 Polyphenylene Ether + Styrene-Butadiene Blend Grade with high resistance to heat deformation and outstanding impact strength. For auto parts such as air vents or the instrument panel; also used for door-mirror housings.Data was collected by IS.. |