Physical Properties | Metric | English | Comments |
---|---|---|---|
High Load Melt Index | 42 g/10 min @Load 21.6 kg, Temperature 190 °C |
42 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Braskem BU 004 HDPE Blow Molding Polyethylene Applications: Bottles for food products, lubricating and cooking oil; toys; bottler for surface-active agents; sheets. Information provided by Braskem |