Physical Properties Metric English Comments
Surface Tension 54 dynes/cm
54 dynes/cm
Solvay Specialty Polymers Diofan® A610 Polyvinylidene Chloride (PVDC)  (discontinued **)
DIOFAN® A610 is a water based dispersion of a polyvinylidene chloride copolymer. It is free of solvent traces, alkylphenol ethoxylates or any other toxic substances. It features exceptional barrier..