Physical Properties | Metric | English | Comments |
---|---|---|---|
Surface Tension | 34 - 36 dynes/cm | 34 - 36 dynes/cm | 2nd surface; units: Dyne; Dyne Pens |
SABIC Innovative Plastics Valox® FR1 Polybutylene Terephthalate Film, Flame Retardant Valox FR-1 film is a flame retardant thermoplastic polybutylene, terephthalite film offering UL94 VTM-0 performance down to 125 microns and good temperature performance. Valox FR-1 film’s outst.. |