Physical Properties Metric English Comments
Surface Tension 34 dynes/cm
34 dynes/cm
25°C
LyondellBasell PMP Propylene glycol methyl ether propionate
Information provided by Lyondell.
Surface Tension 34 - 36 dynes/cm
34 - 36 dynes/cm
2nd surface; units: Dyne; Dyne Pens
SABIC Innovative Plastics Valox® FR1 Polybutylene Terephthalate Film, Flame Retardant
Valox FR-1 film is a flame retardant thermoplastic polybutylene, terephthalite film offering UL94 VTM-0 performance down to 125 microns and good temperature performance. Valox FR-1 film’s outst..
Surface Tension 34 dynes/cm
34 dynes/cm
at CMC
Solvay IGEPAL® CO 710 Surfactant
Chemical Name: NONYLPHENOXY POLY(ETHYLENEOXY)ETHANOL, BRANCHEDCAS: 68412-54-4 Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: IGEPAL© CO-710 is an excellent prima..
Surface Tension 34 dynes/cm
34 dynes/cm
BASF Ecoflex® 1200 F Blend Biodegradable Polyester
Description: A flexible plastic designed for film extrusion and extrusion coating. Ecoflex® F Blend 1200 comes closer than any other biodegradable plastic to the processing properties of LDPE and L..
Surface Tension 34 dynes/cm
34 dynes/cm
Solvay RHODASURF® TR/15-40 Surfactant
Identification: WATER SOLUTION OF ETHOXYLATED TRIDECYL ALCOHOLCAS: 9043 – 30 – 5 ; 7732 – 18 – 5Solubility: Soluble in water and most polar solvents. Insoluble in aromatic solvents.Available in:..
Surface Tension 34 dynes/cm
34 dynes/cm
Solvay RHODOCLEAN® ASP Surfactant
Available in: Asia Pacific, Europe, Latin America and North AmericaSolubility: Soluble in water and most polar solvents. Insoluble in aromatic solvents.Applications: Surfactant for metal working app..