Polymer Property : Surface Tension = 33.0 dynes/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Surface Tension 33.0 - 54.0 dynes/cm
33.0 - 54.0 dynes/cm
Average value: 41.6 dynes/cm Grade Count:5
Overview of materials for Polyvinyl Dichloride (PVDC)
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC)". Each property range of values reported is minimum and maximum values of ap..